Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 14.25 MPa | 2067 psi | after aging 1 week @ 135°C; ASTM D638 |
Trelleborg Horda Cable E6352-A2 Bonded Semiconductive Shielding And Conductor Screen E6352-A2 is a crosslinkable semiconductive compound based on ethylene copolymer compound, designed for conductor screen and insulation shield applications in XLPE and EPDM insulated cables with bond.. |
|||
Tensile Strength, Yield | 14.25 MPa | 2067 psi | after aging 1 week @ 135°C; ASTM D638 |
Trelleborg Horda Cable E7355-A4 Strippable Semiconductive Shielding E7355-A4 is a silane crosslinkable, strippable semiconductive compound for medium voltage cables.E7355-A4 meets the requirements as below, when optimal processing, extrusion and crosslinking procedu.. |
|||
Tensile Strength, Yield | 14.25 MPa | 2067 psi | after aging 1 week @ 135°C; ASTM D638 |
Trelleborg Horda Cable E8900 Strippable Semiconductive Shielding E8900 is a vulcanizable, strippable semiconductive compound, designed for both XLPE and EPDM rubber insulated cables and use in both dry and steam curing processes.E8900 meets the requirements as be.. |