Tensile Strength, Yield 1.39 MPa
202 psi
AVG Stress at Elongation M50; ASTM D412 Method A
Seals Eastern 5242 Neoprene / Chloroprene
General purpose neopreneInformation provided by Seals Eastern, Inc.