Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 20.6 MPa | 2990 psi | ASTM D412 |
Polymax® Maxelast® P3899 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Strength, Yield | 20.6 MPa | 2990 psi | ASTM D638 |
NOVA Chemicals Novapol® TI-0338-A MDPE Masterbatch Resin Molded Plaque Properties. Features: Hexene Copolymer, excellent impact strength, excellent ESCR.Applications: large parts, agricultural storage tanks.Data provided by the manufacturer. |
|||
Tensile Strength, Yield | 20.6 MPa | 2990 psi | ASTM D638 |
NOVA Chemicals Novapol® TR-0338-U MDPE Rotational Molding Resin
(discontinued **) Molded Plaque Properties. Features: Hexene Copolymer, excellent impact strength, excellent ESCR.Applications: large parts, agricultural storage tanks.Data provided by the manufacturer. |
|||
Tensile Strength, Yield | 20.6 MPa @Thickness 3.20 mm |
2990 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LUPOL HF5157 PP+Rubber+MF, High Flow and Stiffness, High Impact Description: Injection Molding, PP+Rubber+MF, High Flow and Stiffness, High Impact, Good Weatherability, Scratch ResistanceApplication: Automotive Exterior (Slim wall Bumper Fascia)Information provi.. |
|||
Tensile Strength, Yield | 20.6 MPa @Thickness 3.20 mm |
2990 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LUPOL HM3207SM PP+MF30%, High Impact Description: Injection Molding, PP+MF30%, Good Weatherability, High ImpactApplication: Automotive Interior Parts CAS: 9003-07-0, 9010-79-1 and 14807-96-6Information provided by LG Chemical |
|||
Tensile Strength, Yield | 20.6 MPa | 2990 psi | 100% elongation |
Lubrizol Estane® UB601 Thermoplastic Polyurethane Type: Estane® UB601 resin is a linear, hydroxyl terminated polyurethane polymer designed to be used as a binder for ink formulations. For ink applications, it gives high hardness to coated surface.. |
|||
Tensile Strength, Yield | 20.6 MPa | 2990 psi | at 300% elongation; ASTM D412 |
Lubrizol Estane® X-595A-3FR Thermoplastic Polyurethane Type: Estane® X595A-3FR TPU is a Shore 94A, polyester type thermoplastic polyurethane elastomer.Uses: Film Blowing, Extrusion.Available in AsiaInformation Provided by The Lubrizol Corporation |
|||
Tensile Strength, Yield | 20.6 MPa | 2990 psi | |
Zylog Hipolyene® 1533 VW Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Tensile Strength, Yield | 20.6 MPa | 2990 psi | |
Zylog Hipolyene® 5131 RA Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Tensile Strength, Yield | 20.6 MPa | 2990 psi | |
Zylog Hipolyene® 6131 XF Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Tensile Strength, Yield | 20.6 MPa | 2990 psi | |
Zylog Hipolyene® 8110 Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Tensile Strength, Yield | 20.6 MPa @Strain 100 % |
2990 psi @Strain 100 % |
ASTM D638 |
Toyobo A3064D Thermoplastic Polyurethane Elastomer, Injection Grade Polyether type, featuring excellent resistance to hot water and fungus. Various grades of Toyobo polyurethane TPEs are used in auto parts, hoses, tubes, sporting goods, shoe soles, etc.Information .. |
|||
Tensile Strength, Yield | 20.6 MPa | 2990 psi | |
Zylog Hipolyene® 8005 DW Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Tensile Strength, Yield | 20.6 MPa | 2990 psi | ASTM D638 |
NOVA Chemicals Novapol® TR-0338-UG MDPE Rotational Molding Resin
(discontinued **) Molded Plaque Properties. Features: Hexene Copolymer, excellent impact strength, excellent ESCR.Applications: large parts, agricultural storage tanks.Data provided by the manufacturer. |
|||
Tensile Strength, Yield | 20.6 MPa @Strain 100 % |
2990 psi @Strain 100 % |
ASTM D638 |
Toyobo A1061D Thermoplastic Polyurethane Elastomer, Injection Grade Polybutyleneadipate type, the most general purpose type of Toyobo Polyurethane; features excellent cost-performance. Various grades of Toyobo polyurethane TPEs are used in auto parts, hoses, tubes,.. |
|||
Tensile Strength, Yield | 20.6 MPa | 2990 psi | |
Zylog Hipolyene® 8110 EX Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |