Lubrizol Estane® X-595A-3FR Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Estane® X-595A-3FR Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Type: Estane® X595A-3FR TPU is a Shore 94A, polyester type thermoplastic polyurethane elastomer.Uses: Film Blowing, Extrusion.Available in AsiaInformation Provided by The Lubrizol Corporation
Physical Properties Metric English Comments
Specific Gravity 1.22 g/cc
1.22 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 94
94
ASTM D2240
Tensile Strength, Ultimate 39.2 MPa
5690 psi
ASTM D412
Tensile Strength, Yield 11.8 MPa
1710 psi
at 100% elongation; ASTM D412
20.6 MPa
2990 psi
at 300% elongation; ASTM D412
Elongation at Break 550 %
550 %
ASTM D412
Tear Strength 113 kN/m
644 pli
Die C; ASTM D624
Compression Set 15 %

@Temperature 23.0 °C,
Time 79200 sec
15 %

@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395
60 %

@Temperature 70.0 °C,
Time 79200 sec
60 %

@Temperature 158 °F,
Time 22.0 hour
ASTM D395
Thermal Properties Metric English Comments
Vicat Softening Point 105 °C
221 °F
ASTM D1525