Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 2.60 MPa | 377 psi | M100 |
3M Dyneon™ Fluorel™ FE-5730Q Fluoroelastomer VF2 + HFP + TFE Terpolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 69.2%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. 69.2% F grade terpolymer with good pe.. |
|||
Tensile Strength, Yield | 2.60 - 72.2 MPa | 377 - 10500 psi | Average value: 23.7 MPa Grade Count:77 |
Overview of materials for Polyester Thermoplastic Elastomer This property data is a summary of similar materials in the MatWeb database for the category "Polyester Thermoplastic Elastomer". Each property range of values reported is minimum and maximum values.. |
|||
Tensile Strength, Yield | 2.60 MPa | 377 psi | At 100% elongation, across flow; ASTM D412 |
Advanced Elastomer Systems Santoprene® 8281-65 Thermoplastic Rubber
(discontinued **) Description: A colorable thermoplastic medical grade elastomer. It has USP Class VI Certificate of Compliance for biocompatibility and can be processed using injection molding, extrusion, or other .. |
|||
Tensile Strength, Yield | 2.60 MPa @Strain 100 % |
377 psi @Strain 100 % |
ISO 527 |
A. Schulman INVISION™ VX-5060UI INVISIONTMSoft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-5060UI is a UV-stabilized polyolefin-based thermoplastic elastomer of 60 Shore A durometer, which has been formulated for easy moldability, soft touch, low gloss, and excell.. |
|||
Tensile Strength, Yield | 2.60 MPa @Strain 100 % |
377 psi @Strain 100 % |
ISO 527 |
A. Schulman INVISION™ VX-5060UI INVISIONTMSoft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-5060UI is a UV-stabilized polyolefin-based thermoplastic elastomer of 60 Shore A durometer, which has been formulated for easy moldability, soft touch, low gloss, and excell.. |
|||
Tensile Strength, Yield | 2.60 MPa @Strain 100 % |
377 psi @Strain 100 % |
ISO 527 |
A. Schulman INVISION™ VX-5060UI INVISIONTMSoft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-5060UI is a UV-stabilized polyolefin-based thermoplastic elastomer of 60 Shore A durometer, which has been formulated for easy moldability, soft touch, low gloss, and excell.. |
|||
Tensile Strength, Yield | 2.60 MPa @Strain 100 % |
377 psi @Strain 100 % |
ISO 527 |
A. Schulman INVISION™ VX-5060UI INVISIONTMSoft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-5060UI is a UV-stabilized polyolefin-based thermoplastic elastomer of 60 Shore A durometer, which has been formulated for easy moldability, soft touch, low gloss, and excell.. |
|||
Tensile Strength, Yield | 2.60 MPa @Strain 100 % |
377 psi @Strain 100 % |
ISO 527 |
A. Schulman INVISION™ VX-5060UI INVISIONTMSoft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-5060UI is a UV-stabilized polyolefin-based thermoplastic elastomer of 60 Shore A durometer, which has been formulated for easy moldability, soft touch, low gloss, and excell.. |
|||
Tensile Strength, Yield | 2.60 MPa @Strain 100 % |
377 psi @Strain 100 % |
ISO 527 |
A. Schulman INVISION™ VX-5060UI INVISIONTMSoft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-5060UI is a UV-stabilized polyolefin-based thermoplastic elastomer of 60 Shore A durometer, which has been formulated for easy moldability, soft touch, low gloss, and excell.. |
|||
Tensile Strength, Yield | 2.60 MPa | 377 psi | ASTM D638 |
Arkema Group OREVAC® 9304 EVA Terpolymer OREVAC® is a range of ethylene-vinyl acetate copolymers modified by adjunction of polar groups which, when molten, have excellent adhesive properties to various substrates. They are supplied as fre.. |
|||
Tensile Strength, Yield | 2.60 - 4.00 MPa @Temperature 70.0 - 100 °C |
377 - 580 psi @Temperature 158 - 212 °F |
Average value: 3.43 MPa Grade Count:1 |
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyester Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyester Grade". Each property range of values reported is minimum a.. |