Polymer Property : Tensile Strength, Yield = 18.60 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 18.60 MPa
2698 psi
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 1.5 PHR Thanecure® ZM
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
Tensile Strength, Yield 18.60 MPa
2698 psi
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 1.5 PHR Thanecure® ZM
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
Tensile Strength, Yield 18.60 MPa
2698 psi
ASTM D638
DuPont Surlyn® PC2000  (discontinued **)
DuPont™ Surlyn® PC2000 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The high MAA c..