Material Notes:
DuPont™ Surlyn® PC2000 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The high MAA content and mid-range neutralization level for this grade creates an exceptional combination of strengths: toughness, low-temperature toughness, abrasion resistance, tear resistance, excellent clarity, and high stiffness compared with other grades of Surlyn®. The resin is highly suitable for injection molding, providing enhanced processability over other grades. Surlyn ® PC2000 is ideal for applications where easy melt flow characteristics and high stiffness, high clarity and good abrasion resistance are desired. In golf ball covers, it provides good cut resistance, impact durability, high resiliency and increased coefficient of restitution, particularly when used in blends with different cations.Information provided by DuPont™
Physical Properties Metric English Comments
Density 0.970 g/cc
0.0350 lb/in³
ASTM D792-ISO 1183
Melt Flow 4.5 g/10 min

@Load 2.16 kg
4.5 g/10 min

@Load 4.76 lb
Condition E; ASTM D1238, ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
ASTM D2240-ISO 868
Tensile Strength at Break 31.00 MPa
4496 psi
ASTM D638 ISO 527-2
Tensile Strength, Yield 18.60 MPa
2698 psi
ASTM D638
Elongation at Break 320 %
320 %
ASTM D638 ISO 527-2
Flexural Modulus 0.490 GPa
71.1 ksi
ASTM D790
Tensile Impact Strength 897 kJ/m²
427 ft-lb/in²
ASTM D1822
Abrasion 301
301
NBS Index; ASTM D1630
Thermal Properties Metric English Comments
Melting Point 104 °C
219 °F
Freezing Point; ASTM D3418
183 °C
361 °F
ASTM D3417- ISO 3146
Vicat Softening Point 127 °C
261 °F
ASTM D1525, ISO 306
Optical Properties Metric English Comments
Haze 1.3 %
1.3 %
ASTM D1003