Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1793 MPa @Strain 0.200 % |
260100 psi @Strain 0.200 % |
|
AK Steel 17-7 PH® Precipitation Hardening Stainless Steel, Condition CH 900 AK Steel 17-7 PH® provides high strength and hardness, excellent fatigue properties, good corrosion resistance, good formability, and minimum distortion upon heat treatment. This alloy provides va.. |
|||
Tensile Strength, Yield | 1793 MPa @Strain 0.200 % |
260100 psi @Strain 0.200 % |
|
Carpenter AerMet®-for-Tooling Tool Steel, Double Aged 468°C Data provided by Carpenter Technology Corporation.This is a double vacuum melted alloy with high hardness and strength combined with exceptional ductility and toughness. The alloy is designed for c.. |
|||
Tensile Strength, Yield | 1793 MPa @Strain 0.200 % |
260100 psi @Strain 0.200 % |
|
AK Steel PH 15-7 Mo® Precipitation Hardening Stainless Steel, Condition CH 900 AK Steel 15-7 Mo® provides high strength and hardness, good corrosion resistance and minimum distortion on heat treatment. It is easily formed in the annealed condition and develops effective bala.. |