Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 71.0 - 174 MPa | 10300 - 25200 psi | Average value: 111 MPa Grade Count:5 |
Overview of materials for Polyphthalamide (PPA), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Mineral Filled". Each property range of values reported is minimum and maximum values o.. |