Mechanical Properties Metric English Comments
Tensile Strength, Yield 1160 - 1270 MPa
169000 - 184000 psi
3/4"x 0.030" Fiberglass Reinforced
Glastic GoldMemberâ„¢ Pre-tensioned Fiber Reinforcements
GoldMemberâ„¢ fiber reinforcements are available in ribbon, tape and rounds that can be applied to thermoplastics and thermoset plastics, as well as wood and metals to add strength, rigidity, and..
Tensile Strength, Yield 1165 - 1172 MPa

@Strain 0.200 %
169000 - 170000 psi

@Strain 0.200 %
Latrobe Lescalloy® UT-18 VAC-ARC ; 3.75 in. round High Strength Alloy Steel
UT-18 VAC-ARC is a medium-carbon, low-alloy heat resistant steel having high strength to 1000°F. It is used primarily for turbine and compressor rotor shafts. Vacuum consumable electrode melting..
Tensile Strength, Yield 1165 MPa

@Strain 0.200 %
169000 psi

@Strain 0.200 %
Carpenter Custom 450® Stainless Steel, Condition H1000 (Age Hardened 538°C (1000°F))
Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T..