Polymer Property : Tensile Strength, Yield = 161 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 161 MPa
23400 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP LX91475 PEEK
LNP* LUBRICOMP* LX91475 is a compound based on Polyetheretherketone resin containing proprietary fillers. Added features of this material include: Easy Molding, High Temperature Bearing Grade, Wear..
Tensile Strength, Yield 161 MPa
23400 psi
ASTM D638
Techmer ES HiFill® PEI GF30 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightInformation provided by TP Composites, Inc.
Tensile Strength, Yield 161 MPa
23400 psi
ISO 527
Eurostar Star L PA66 15Y D52 PA66, Carbon Filled, Injection Molded
Star L PA66 15Y D52 is a PTFE Lubricated, Carbon Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar.
Tensile Strength, Yield 161 MPa
23400 psi
ASTM D638
Techmer ES HiFill FR® PA6/6 GF25 FR NAT005 25% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 25% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Heat Stabilized, High Flow and Lubri..