Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1552 MPa @Temperature 24.0 °C |
225100 psi @Temperature 75.2 °F |
|
Hexcel® HexPly® F155 Epoxy Resin, T3T095 Carbon Tape Hexcel designation: TXX095-12"-F155; Various fibersInformation provided by HexCel |
|||
Tensile Strength, Yield | 1552 MPa @Strain 0.200 % |
225100 psi @Strain 0.200 % |
|
AK Steel PH 15-7 Mo® Precipitation Hardening Stainless Steel, Condition RH 950 AK Steel 15-7 Mo® provides high strength and hardness, good corrosion resistance and minimum distortion on heat treatment. It is easily formed in the annealed condition and develops effective bala.. |