Polymer Property : Tensile Strength, Yield = 1527 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 10.53 MPa
1527 psi
-35% change after 72 hours @ 250°C; ASTM D412
Precision Polymer Engineering Perlast® G70G Green Perfluoroelastomer
Excellent chemical resistance, steam resistance and good mechanical properties. Color coded for identification.Applications: Specially developed for critical applications where good chemical resista..
Tensile Strength, Yield 10.53 MPa
1527 psi
AVG Stress at Elongation M100; ASTM D412 Method A
Seals Eastern 7168 Nitrile Rubber
Nitrile for oil & gas serviceInformation provided by Seals Eastern, Inc.