Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 10.53 MPa | 1527 psi | -35% change after 72 hours @ 250°C; ASTM D412 |
Precision Polymer Engineering Perlast® G70G Green Perfluoroelastomer Excellent chemical resistance, steam resistance and good mechanical properties. Color coded for identification.Applications: Specially developed for critical applications where good chemical resista.. |
|||
Tensile Strength, Yield | 10.53 MPa | 1527 psi | AVG Stress at Elongation M100; ASTM D412 Method A |
Seals Eastern 7168 Nitrile Rubber Nitrile for oil & gas serviceInformation provided by Seals Eastern, Inc. |