Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1500 MPa | 218000 psi | |
ThyssenKrupp XAR® 550 Structural Steel This Material Specification applies to 4 to 100 mm thick plates of the wear-resistant special structural steel XAR® 550.Application: The steel may be used for wear exposed structures, e.g. excavati.. |
|||
Tensile Strength, Yield | 1500 MPa | 218000 psi | |
ThyssenKrupp XAR® SUPRA Structural Steel This Material Specification applies to 4 to 100 mm thick plates of the wear-resistant special structural steel XAR® SUPRA.Application: The steel may be used for wear exposed structures, e.g. excava.. |
|||
Tensile Strength, Yield | 1500 MPa | 218000 psi | |
ThyssenKrupp SECURE 600 Structural Steel This Material Specification applies to the alloyed, liquid-quenched and tempered high-strength special steel SECURE 600 for civil use, that is usually produced from 4 up to 40 mm in thickness.Applic.. |
|||
Tensile Strength, Yield | 1500 MPa | 218000 psi | EN2561 |
Hexcel® HexPly® M52 120°C/250°F Curing Epoxy, M52/38%/UD150/CHS/460mm Fiber mass: 150 g/m2Information provided by HexCel |
|||
Tensile Strength, Yield | 1500 MPa @Strain 0.200 % |
218000 psi @Strain 0.200 % |
|
Carpenter Extendo-Die® Hot Work Die Steel, Tempered 593°C Data provided by Carpenter Technology Corporation.This steel combines extreme toughness with good red hardness in large section sizes. This alloy may also be considered for many cold work applicati.. |