Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 15.58 MPa | 2260 psi | ASTM D412 |
Precision Polymer Engineering C60W Chloroprene Rubber Off-white, Chloroprene Rubber, 56-65 °IRHDApplications: A versatile rubber with good compression set properties, giving moderate resistance to petroleum based oils, ozone and weather. |