Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Precision Polymer Engineering C60W Chloroprene Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Chlorosulfonated Polyethylene Rubber
Manufacturer Precision Polymer Engineering Limited
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Precision Polymer Engineering C60W Chloroprene Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Off-white, Chloroprene Rubber, 56-65 °IRHDApplications: A versatile rubber with good compression set properties, giving moderate resistance to petroleum based oils, ozone and weather.
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
°IRHD; ASTM D1415
70
70
°IRHD, +10 change after 168 hours @ 70°C; ASTM D1415
Tensile Strength, Yield 13.243 MPa
1920.7 psi
-15% change after 168 hours @ 70°C; ASTM D412
15.58 MPa
2260 psi
ASTM D412
Elongation at Break 487.5 %
487.5 %
-35% change after 168 hours @ 70°C; ASTM D412
750 %
750 %
ASTM D412
Compression Set 31 %
31 %
24 hours @ 70°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 125 °C
257 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
-40.0 °C
-40.0 °F
Non-brittle after 3 minutes
Flash Point >= 260 °C
>= 500 °F