Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1018 MPa @Strain 0.200 % |
147600 psi @Strain 0.200 % |
|
International Mold Steel NAK80 Precipitation Hardened Mold Steel Description: NAK80 is a precipitation or age-hardened mold steel with a uniform through hardness of approximately 40 HRc. It is super clean, Vacuum-Arc Remelted steel with uniform grain structure, u.. |