Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1010 MPa @Strain 0.200 % |
146500 psi @Strain 0.200 % |
|
International Mold Steel NAK55 Precipitation Hardened Mold Steel Description: NAK55 is a precipitation, or age-hardened mold steel with a through hardness of approximately 40 HRc. NAK55 is ideal for use in plastic and rubber molds and other applications where imp.. |