Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 9.60 MPa | 1390 psi | -20% change after 70 hours @ 125°C; ASTM D412 |
Precision Polymer Engineering E80V Ethylene Propylene Rubber Peroxide cured, blue-violet coloured Ethylene Propylene Terpolymer, 75-85 °IRHD. Terpolymer of ethylene, propylene and diene monomers. Specially formulated for sealing applications involving high.. |
|||
Tensile Strength, Yield | 9.60 MPa | 1390 psi | ASTM D638 |
DuPont 20 Series 2020 Specialty Polyethylene Resin
(discontinued **) DuPont 2020T and 2020 specialty low density polyethylene resins are products characterized by low melt index and intermediate crystallinity. These products, produced via a unique polymerization proc.. |
|||
Tensile Strength, Yield | 9.60 MPa | 1390 psi | ASTM D638 |
DuPont 20 Series 2010 Specialty Polyethylene Resin DuPont 2010 specialty low density polyethylene resin is characterized by low melt index and intermediate crystallinity. This product, produced via a unique polymerization process, has outstanding fl.. |
|||
Tensile Strength, Yield | 9.60 MPa | 1390 psi | ASTM D638 |
DuPont 20 Series 2020T Specialty Polyethylene Resin DuPont 2020T and 2020 specialty low density polyethylene resins are products characterized by low melt index and intermediate crystallinity. These products, produced via a unique polymerization proc.. |
|||
Tensile Strength, Yield | 9.60 MPa | 1390 psi | ASTM D638 |
DuPont 20 Series 20-6064 Specialty Polyethylene Resin DuPont 20-6064 specialty low density polyethylene resin is characterized by low melt index and intermediate crystallinity. This product, produced via a unique polymerization process, has outstanding.. |
|||
Tensile Strength, Yield | 9.60 MPa | 1390 psi | ASTM D638 |
DuPont 20 Series DPE 20 Specialty Polyethylene Resin DuPont 20 specialty low density polyethylene resin is characterized by low melt index and intermediate crystallinity. This product, produced via a unique polymerization process, has outstanding flex.. |
|||
Tensile Strength, Yield | 9.60 MPa @Treatment Temp. 200 °C, Time 252000 sec |
1390 psi @Treatment Temp. 392 °F, Time 70.0 hour |
Heat Aging; ASTM D573 |
Vicone High Performance Rubber VicoSil™ C240Q-RD High Performance Silicone Rubber Information provided by Vicone |
|||
Tensile Strength, Yield | 9.60 MPa | 1390 psi | |
Dow DOWLEX™ 2505 Linear Low Density Polyethylene, Narrow MW Distribution DOWLEX® 2505 Polyethylene resin is a narrow molecular weight distribution copolymer designed to offer excellent environmental stress crack resistance and tear strength with good rigidity. It has ex.. |
|||
Tensile Strength, Yield | 9.60 MPa @Strain 50.0 % |
1390 psi @Strain 50.0 % |
|
Covestro Texin® 250 Urethane Thermoplastic Elastomer Key Features:UnfilledSuitable processing methods:Injection moldingProfile extrusionSheet extrusionCoatingBlow moldingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScie.. |