Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 0.951 MPa | 138 psi | ASTM D412 |
Polymax® Maxelast® C4803 TPE, Transparent Characteristics:Excellent clarityOvermold adhesion to polypropyleneUltrasoft TPEs with gel-like propertiesSoft and cushioning comfortSuperior colorabilityPVC, silicone, and latex freeTypical Applica.. |
|||
Tensile Strength, Yield | 0.951 MPa | 138 psi | AVG Stress at Elongation M25; ASTM D412 Method A |
Seals Eastern 7017 Ethylene-Propylene Rubber General service EPM.Information provided by Seals Eastern, Inc. |
|||
Tensile Strength, Yield | 0.951 MPa | 138 psi | AVG Stress at Elongation M25; ASTM D412 Method A |
Seals Eastern 7017 Ethylene-Propylene Rubber General service EPM.Information provided by Seals Eastern, Inc. |