Polymax® Maxelast® C4803 TPE, Transparent

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Nagtong Polymax
Trade Name Maxelast®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polymax® Maxelast® C4803 TPE, Transparent.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Characteristics:Excellent clarityOvermold adhesion to polypropyleneUltrasoft TPEs with gel-like propertiesSoft and cushioning comfortSuperior colorabilityPVC, silicone, and latex freeTypical Applications:ConsumerPackagingHealthcareElectronicsInformation from Alliance Polymers & Services, Distributor of Nantong Elastomer Technology Co.Ltd
Physical Properties Metric English Comments
Specific Gravity 0.822 g/cc
0.822 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 3.0
3.0
ASTM D2240
Tensile Stress 0.0903 MPa

@Strain 100 %
13.1 psi

@Strain 100 %
ASTM D412
0.190 MPa

@Strain 300 %
27.6 psi

@Strain 300 %
ASTM D412
Tensile Strength, Yield 0.951 MPa
138 psi
ASTM D412
Elongation at Break 910 %
910 %
ASTM D412