Polymer Property : Tensile Strength, Yield = 13.243 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 13.243 MPa
1920.7 psi
-15% change after 168 hours @ 70°C; ASTM D412
Precision Polymer Engineering C60W Chloroprene Rubber
Off-white, Chloroprene Rubber, 56-65 °IRHDApplications: A versatile rubber with good compression set properties, giving moderate resistance to petroleum based oils, ozone and weather.