Mechanical Properties Metric English Comments
Tensile Strength, Yield 0.866 MPa
126 psi
ASTM D638
Cheng Yu Plastic E2345 Flame Retardant PET, 45% Glass Fiber
Tensile Strength, Yield 0.866 - 195 MPa
126 - 28300 psi
Average value: 138 MPa Grade Count:9
Overview of materials for Polyethylene Terephthalate (PET), 50% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 50% Glass Reinforced". Specific grades with glass content between 45% ..