Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 0.866 MPa | 126 psi | ASTM D638 |
Cheng Yu Plastic E2345 Flame Retardant PET, 45% Glass Fiber |
|||
Tensile Strength, Yield | 0.866 - 195 MPa | 126 - 28300 psi | Average value: 138 MPa Grade Count:9 |
Overview of materials for Polyethylene Terephthalate (PET), 50% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 50% Glass Reinforced". Specific grades with glass content between 45% .. |