Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 0.814 MPa | 118 psi | AVG Stress at Elongation M50; ASTM D412 Method A |
Seals Eastern 5241 Neoprene / Chloroprene General purpose neopreneInformation provided by Seals Eastern, Inc. |