Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1138 - 1172 MPa @Strain 0.200 % |
165100 - 170000 psi @Strain 0.200 % |
Core heat treated from 1850°F |
Latrobe CBS-223â„¢ VIM-VAR Carburizing Bearing and Gear Steel CBS-223 VIM-VAR steel is a double vacuum melted carburizing steel with high hot hardness characteristics. Double vacuum melting sequentially combines vacuum induction melting with VACARCâ„¢ remel.. |
|||
Tensile Strength, Yield | 1138 MPa @Strain 0.200 % |
165100 psi @Strain 0.200 % |
|
ATI Allvac® Vasco® X-2M Specialty Steel, Heat Treatment: 899°C (1650°F) Normalization Data provided by Allvac.Applications: High performance helicopter transmission gears, components. |
|||
Tensile Strength, Yield | 1138 MPa @Strain 0.200 % |
165100 psi @Strain 0.200 % |
|
ATI Allegheny Ludlum AL 13-8™ H 1050 Precipitation Hardening Alloy, Heat Treated at 1050°F Characteristics: excellent strength, high hardness, superior toughness, good corrosion resistance, good transverse toughness properties, strength and ductility can be tailored by varying the aging t.. |