Polymer Property : Tensile Strength, Yield = 113 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 0.779 MPa
>= 113 psi
Stress at Elongation M50; ASTM D412 Method A
Seals Eastern 7240 Ethylene-Propylene Rubber
Potable water service. Chloramine resistant.Information provided by Seals Eastern, Inc.