Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 662 - 765 MPa | 96000 - 111000 psi | 0.2% offset |
Eagle Brass 519 Phosphor Bronzes 6%, Spring Alloy C519 has 6% nominal tin producing higher mechanical strengths with a slight decrease in electrical conductivity when compared to C510 phosphor bronze. Often functionally interchangeable with C.. |