Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 552 - 724 MPa @Strain 0.200 %, Thickness <=25.4 mm |
80000 - 105000 psi @Strain 0.200 %, Thickness <=1.00 in |
Cold Drawn Bars |
Schmolz + Bickenbach 416 Stainless Steel Bar Description: Ugitech’s 416 is free machining martensitic grade. The unique production process—developed exclusively by Ugitech—results in a product that delivers superior productivity.. |