Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 0.917 MPa
>= 133 psi
Stress at Elongation M100; ASTM D412 Method A
Seals Eastern 5241 Neoprene / Chloroprene
General purpose neopreneInformation provided by Seals Eastern, Inc.