Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 93.0 MPa
13500 psi
ASTM D882
ExxonMobil Escorene® HD-7000F HMW-HDPE Blown Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A high molecular weight HDPE blown film resin. Films made from HD-7000F exhibit excellent impact and toughness properties as well as high stiffness..
Film Tensile Strength at Break, MD 93.0 MPa
13500 psi
ASTM D882
ExxonMobil Escorene® HD-7745 HMW-HDPE Blown Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A high molecular weight HDPE blown film resin. Films made from HD-7745 exhibit excellent impact and toughness properties as well as high stiffness...
Film Tensile Strength at Break, MD 93.0 MPa
13500 psi
ASTM D882
ExxonMobil Escorene® HDZ-123 HMW-HDPE Blown Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A high molecular weight HDPE blown film resin. Films made from HDZ-123 exhibit excellent impact and toughness properties as well as high stiffness...