Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 62.0 MPa | 8990 psi | |
Premix Thermoplastics PREFLEX E25 Polyphenylene Ether (PPO/PPE) PREFLEX films combine outstanding dielectric properties, good heat stability, low water absorption and chemical resistance in a way not available before. Also rigid boards made of the same material .. |
|||
Film Tensile Strength at Break, MD | 62.0 MPa | 8990 psi | ASTM D882 |
DuPont™ Clysar® LE Polyolefin Shrink Packaging Film, 60 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, heat-shrinkable, multilayer film with the lowest shrink force available in the Clysar® line. Dupont Clysar® LES is .. |
|||
Film Tensile Strength at Break, MD | 62.0 MPa | 8990 psi | ASTM D882 |
DuPont™ Clysar® LE Polyolefin Shrink Packaging Film, 75 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, heat-shrinkable, multilayer film with the lowest shrink force available in the Clysar® line. Dupont Clysar® LES is .. |
|||
Film Tensile Strength at Break, MD | 62.0 MPa | 8990 psi | ASTM D882 |
DuPont™ Dartek® B-601 Nylon 6,6 Barrier Film, 25 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.A strong transparent nylon type 6,6 film which has a PVDC coating applied to one side for enhanced barrier to oxygen, moisture, grease and odor. Can be pri.. |
|||
Film Tensile Strength at Break, MD | 62.0 MPa | 8990 psi | ASTM-D882 |
Westlake Mxsten CV77519 Polyethylene Plastomer Mxsten CV Plastomer CV77519 is a polyethylene plastomer designed for blown film extrusion that contains no slip and no antiblock. It does contain high processing aid. Films produced with this resin .. |
|||
Film Tensile Strength at Break, MD | 62.0 MPa | 8990 psi | ISO 527-3 |
Total PPH 4026 Polypropylene Homopolymer, Film Polypropylene PPH 4026 is a homopolymer polypropylene with a Melt Flow index of 3 g/10 min for the cast extrusion of films with outstanding stiffness and heat resistance.Polypropylene PPH 4026 is in.. |