Polymer Property : Film Tensile Strength at Break, MD = 8800 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 60.7 - 107 MPa
8800 - 15500 psi
ASTM D882
Honeywell Halar® High Performance E-CTFE Film  (discontinued **)
Description: Halar® is a high performance Ethylene-Chlorotrifluoroethylene (E-CTFE) film with excellent mechanical, electrical and release properties. It is non-flammable, and has outstanding chem..
Film Tensile Strength at Break, MD 60.7 MPa
8800 psi
ASTM D882
LyondellBasell Alathon® M6010SB High Density Polyethylene, MMW Film Grade
Alathon M6010SB is a medium molecular weight high density polyethylene homopolymer for use in blown film applications. Typical applications include those with low WVTR requirements. Regulatory Statu..
Film Tensile Strength at Break, MD 60.7 MPa
8800 psi
ASTM D882
ExxonMobil Enable™ 20-10CB Metallocene Polyethylene Resin (European Grade)
Product Description: Enable 20-10 resins are metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact ..
Film Tensile Strength at Break, MD 60.7 MPa
8800 psi
ASTM D882
ExxonMobil Enable™ 20-10CE Metallocene Polyethylene Resin (Africa & Middle East Grade)
Product Description: Enable 20-10 resins are metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact ..
Film Tensile Strength at Break, MD 60.7 MPa
8800 psi
Calculated from mfr's report of 57 N/cm per ASTM D828 and the typical thickness
DuPont™ Nomex® 414 Paper, 3.4 mil Nominal Thickness
Nomex® Type 414 is designed for uses requiring a strong, yet flexible and conformable sheet. It is electrically and thermally similar to Type 410. Type 414 was designed as slot insulation in hand..
Film Tensile Strength at Break, MD 60.7 MPa
8800 psi
ASTM D882
ExxonMobil Enable™ 20-10CH Metallocene Polyethylene Resin (Africa & Middle East Grade)
Product Description: Enable 20-10 resins are metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact ..