Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 86.9 MPa
12600 psi
ASTM D882
Solvay Specialty Polymers Ajedium™ Films -- AvaSpire® AV-630 Polyaryletherketone (PAEK)
AvaSpire® AV-630 PAEK film is a unique thermoplastic film that is characterized by a distinct combination of properties, which include strength, ductility, fatigue resistance, high purity and exc..