Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 83.9 MPa | 12200 psi | Calculated from mfr's report of 341 N/cm per ASTM D828 and the typical thickness |
DuPont™ Nomex® 414 Paper, 15 mil Nominal Thickness Nomex® Type 414 is designed for uses requiring a strong, yet flexible and conformable sheet. It is electrically and thermally similar to Type 410. Type 414 was designed as slot insulation in hand.. |