Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 83.9 MPa | 12200 psi | Calculated from mfr's report of 341 N/cm per ASTM D828 and the typical thickness |
DuPont™ Nomex® 414 Paper, 15 mil Nominal Thickness Nomex® Type 414 is designed for uses requiring a strong, yet flexible and conformable sheet. It is electrically and thermally similar to Type 410. Type 414 was designed as slot insulation in hand.. |
|||
Film Tensile Strength at Break, MD | 84.0 MPa | 12200 psi | ASTM D882 |
Braskem HF 0147 HDPE Blown Film Extrusion Polyethylene 38µm film gauge, obtained in 75mm extruder, die gap 1.0mm, output 1.75 kg/h-cm with 2:1 BUR. Applications: Grocery and T-shirt bags; merchandise bags; frozen-food bags. Information provided by Bras.. |