Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 52.4 MPa
7600 psi
ASTM D882
Chevron Phillips MarFlex® 7109S LLDPE Blown Film Resin  (discontinued **)
Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,..
Film Tensile Strength at Break, MD 52.4 MPa
7600 psi
ASTM D882
Chevron Phillips MarFlex® 7109 LLDPE Blown Film Resin
Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,..
Film Tensile Strength at Break, MD 52.4 MPa
7600 psi
ASTM D882
ExxonMobil Exceed™ 1023JA Metallocene Polyethylene Resin
Product Description: Exceed 1023JA is a metallocene ethylene-hexene copolymer. Films made from Exceed 1023JA have outstanding tensile, impact strength and puncture. These superior strength propertie..
Film Tensile Strength at Break, MD 52.4 MPa
7600 psi
ASTM D882
Dow DOWLEX™ 2020G Linear Low Density Polyethylene
DOWLEX™ 2020G is perfect for high strength consumer trash bags/liners. This product can be used in other applications that require toughness and also offers great melt strength for high throughput..
Film Tensile Strength at Break, MD 52.4 MPa
7600 psi
ASTM D882
M. Holland Company MAGMA® LM311-D LLDPE  (discontinued **)
Features: Good Processability, Good Puncture Resistance, Good Tear Strength, Good ToughnessProcessing Method: ExtrusionInformation provided by M. Holland.