Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 75.2 MPa | 10900 psi | 20 in/min, 2.0 in Jaw Separation; ExxonMobil Method |
ExxonMobil Metallyte™ UHB 35 MWHB OPP Film Product Description: A multi-layer, cavitaed, white OPP film structure that has exceptional barrier to gases and flavors. It is metalized on one side and treated on the other. It is designed for use.. |