Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 68.0 MPa
9860 psi
ASTM D882
ExxonMobil Exceed™ 357C32 LDPE/Hexene Premium Cast Stretch Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A hexene copolymer produced using Exxon Chemical's EXXPOL® technology. Films made from EXCEED 357C32 resin have outstanding tensile properties and..