Polymer Property : Film Tensile Strength at Break, MD = 55.5 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 55.5 MPa
8050 psi
Calculated from mfr's report of 28.2 N/cm per ASTM D828 and the typical thickness
DuPont™ Nomex® N196 Paper, 2 mil Nominal Thickness
Nomex® Type N196 is a high floc grade of Nomex® paper. This leads to a high degree of saturability combined with high stiffness and mechanical properties. Type N196 is used where good saturabili..
Film Tensile Strength at Break, MD 55.5 MPa
8050 psi
25.4 microns; ASTM D882
Dow 118.01 Developmental Performance Polypropylene Polymer
D118.01 Developmental Performance Polymer is a propylene-based resin intended for use in film, sheet extrusion and injection molding applications. Film and sheet produced from this resin offer impr..
Film Tensile Strength at Break, MD 55.5 MPa
8050 psi
ASTM D882
ExxonMobil LL 3201.22 Premium High Strength Film Resin  (discontinued **)
LL 3201 resins are hexene copolymer LLDPE film resins. Films produced from these resins have excellent tensile, toughness and stiffness properties. These strength properties, along with good drawdow..