Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 37.2 MPa | 5400 psi | ASTM D882 |
ExxonMobil Escorene® LD 721.IK Film Resin Escorene Ultra LD 721 is a high vinyl acetate copolymer specialty film resin providing outstanding heat sealability, along with excellent strength properties and clarity.Availability: Latin America,.. |
|||
Film Tensile Strength at Break, MD | 37.2 MPa | 5400 psi | ASTM D882 |
ExxonMobil Paxon™ 4700 Blown Film Extrusion Resin
(discontinued **) 4700 is a medium molecular weight, high density polyethylene homopolymer film resin. It can be processed on conventional film extrusion equipment.Information provided by ExxonMobil Chemical |