Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 24.2 MPa | 3510 psi | ASTM D882 |
ExxonMobil OPTEMA™ TC 115 Blown Film Resin
(discontinued **) OPTEMA TC 115 is an ethylene methyl acrylate copolymer, designed for specialty blown film applications. It yields soft, elastic films.Information provided by ExxonMobil Chemical |
|||
Film Tensile Strength at Break, MD | 24.2 MPa | 3510 psi | ASTM D882 |
ExxonMobil LD 302.20 High Clarity, High Impact Film Resin LD 302 Series films exhibit superior impact strength, good heat sealability, and good low temperature properties. Typical applications are frozen food packaging or other food packaging.Information .. |
|||
Film Tensile Strength at Break, MD | 24.2 MPa | 3510 psi | ASTM D882 |
ExxonMobil LD 302.32 High Clarity, High Impact Film Resin LD 302 Series films exhibit superior impact strength, good heat sealability, and good low temperature properties. Typical applications are frozen food packaging or other food packaging.Information .. |
|||
Film Tensile Strength at Break, MD | 24.2 MPa | 3510 psi | ASTM D882 |
ExxonMobil LD 302.34 High Clarity, High Impact Film Resin LD 302 Series films exhibit superior impact strength, good heat sealability, and good low temperature properties. Typical applications are frozen food packaging or other food packaging.Information .. |
|||
Film Tensile Strength at Break, MD | 24.2 MPa | 3510 psi | ASTM D882 |
ExxonMobil LD 302.56 High Clarity, High Impact Film Resin LD 302 Series films exhibit superior impact strength, good heat sealability, and good low temperature properties. Typical applications are frozen food packaging or other food packaging.Information .. |
|||
Film Tensile Strength at Break, MD | 24.2 MPa | 3510 psi | |
Dow LDPE 493A Low Density Polyethylene, Film Grade DOW LDPE 493A resin, is a high strength, general purpose resin used for shipping sack, industrial liner and produce film applications. DOW LDPE 493A resin can be blended with most linear low density.. |