Polymer Property : Film Tensile Strength at Break, MD = 3420 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 23.6 MPa
3420 psi
ASTM D882
ExxonMobil LD 129.24 Cast Overwrap Film Resin
Product Description: LD 129.24 is a medium density homopolymer film resin with good clarity and excellent stiffness. Film made from LD 129.24 can be used in overwrap applications and in push-through..