Polymer Property : Film Tensile Strength at Break, MD = 31.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 15.0 - 31.0 MPa
2180 - 4500 psi
Average value: 24.0 MPa Grade Count:12
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade". Each property range of values reported..