Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 186.0 MPa | 26970 psi | ASTM D882A |
DuPont Teijin Films Teijin® Tetoron® HSL Polyester Film, 700 Gauge Teijin® Tetoron® HSL is a low shrinkage polyester film with well balanced physical, chemical and optical properties. In addition to the standard, non-pretreated, Teijin® Tetoron® HSL film, the f.. |
|||
Film Tensile Strength at Break, MD | 186.0 MPa | 26970 psi | ASTM D882A |
DuPont Teijin Films Teijin® Tetoron® OWF Polyester Film, 740 Gauge Teijin® Tetoron® O is the designation for a family of super clear polyester films. They have very smooth surface characteristics and are knurled. The combination of smoothness and knurling provide.. |
|||
Film Tensile Strength at Break, MD | 186.0 MPa | 26970 psi | ASTM D882A |
DuPont Teijin Films Teijin® Tetoron® U4 Polyester Film, 100 Gauge Teijin® Tetoron® U4 is a filled, translucent white polyester film. It has rough surface characteristics.This film is also available pretreated for slip - known as Teijin® Tetoron® U4Z. This prod.. |
|||
Film Tensile Strength at Break, MD | 186.0 MPa | 26970 psi | ASTM D882A |
DuPont Teijin Films Teijin® Tetoron® U4 Polyester Film, 150 Gauge Teijin® Tetoron® U4 is a filled, translucent white polyester film. It has rough surface characteristics.This film is also available pretreated for slip - known as Teijin® Tetoron® U4Z. This prod.. |
|||
Film Tensile Strength at Break, MD | 186.0 MPa | 26970 psi | ASTM D882A |
DuPont Teijin Films Teijin® Tetoron® U4 Polyester Film, 400 Gauge Teijin® Tetoron® U4 is a filled, translucent white polyester film. It has rough surface characteristics.This film is also available pretreated for slip - known as Teijin® Tetoron® U4Z. This prod.. |
|||
Film Tensile Strength at Break, MD | 186.0 MPa | 26970 psi | ASTM D882A |
DuPont Teijin Films Teijin® Tetoron® U4 Polyester Film, 63 Gauge Teijin® Tetoron® U4 is a filled, translucent white polyester film. It has rough surface characteristics.This film is also available pretreated for slip - known as Teijin® Tetoron® U4Z. This prod.. |