Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 186.0 MPa
26970 psi
ASTM D882A
DuPont Teijin Films Teijin® Tetoron® HSL Polyester Film, 700 Gauge
Teijin® Tetoron® HSL is a low shrinkage polyester film with well balanced physical, chemical and optical properties. In addition to the standard, non-pretreated, Teijin® Tetoron® HSL film, the f..
Film Tensile Strength at Break, MD 186.0 MPa
26970 psi
ASTM D882A
DuPont Teijin Films Teijin® Tetoron® OWF Polyester Film, 740 Gauge
Teijin® Tetoron® O is the designation for a family of super clear polyester films. They have very smooth surface characteristics and are knurled. The combination of smoothness and knurling provide..
Film Tensile Strength at Break, MD 186.0 MPa
26970 psi
ASTM D882A
DuPont Teijin Films Teijin® Tetoron® U4 Polyester Film, 100 Gauge
Teijin® Tetoron® U4 is a filled, translucent white polyester film. It has rough surface characteristics.This film is also available pretreated for slip - known as Teijin® Tetoron® U4Z. This prod..
Film Tensile Strength at Break, MD 186.0 MPa
26970 psi
ASTM D882A
DuPont Teijin Films Teijin® Tetoron® U4 Polyester Film, 150 Gauge
Teijin® Tetoron® U4 is a filled, translucent white polyester film. It has rough surface characteristics.This film is also available pretreated for slip - known as Teijin® Tetoron® U4Z. This prod..
Film Tensile Strength at Break, MD 186.0 MPa
26970 psi
ASTM D882A
DuPont Teijin Films Teijin® Tetoron® U4 Polyester Film, 400 Gauge
Teijin® Tetoron® U4 is a filled, translucent white polyester film. It has rough surface characteristics.This film is also available pretreated for slip - known as Teijin® Tetoron® U4Z. This prod..
Film Tensile Strength at Break, MD 186.0 MPa
26970 psi
ASTM D882A
DuPont Teijin Films Teijin® Tetoron® U4 Polyester Film, 63 Gauge
Teijin® Tetoron® U4 is a filled, translucent white polyester film. It has rough surface characteristics.This film is also available pretreated for slip - known as Teijin® Tetoron® U4Z. This prod..