Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 17.2 MPa
2500 psi
ASTM D882
LyondellBasell Petrothene® NA336149 Low Density Polyethylene
ApplicationsPETROTHENE NA 336 is a homopolymer resin specifically engineered for garment film and dry cleaning bag applications. This resin is also suitable for any application requiring thin gauge..
Film Tensile Strength at Break, MD 17.2 MPa
2500 psi
ASTM D882
Westlake EF602 Low Density Polyethylene
Westlake EF602 is a fractional melt LDPE with excellent toughness. It is suggested in heavy duty films and shipping sacks, and in industrial shrink applications. It can be used as a bubble stabilize..