LyondellBasell Petrothene® NA336149 Low Density Polyethylene

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Film Grade
Manufacturer LyondellBasell (former Equistar)
Trade Name Petrothene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Petrothene® NA336149 Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ApplicationsPETROTHENE NA 336 is a homopolymer resin specifically engineered for garment film and dry cleaning bag applications. This resin is also suitable for any application requiring thin gauge film constructions. NA 336 is know for its consistency, exceptional drawdown and processability. Regulatory StatusNA 336 meets the requirements of the Food and Drug Administration regulation, 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "…articles or components of articles intended for use in contact with food…" Specific limitations or conditions of use may apply. Contact your Equistar sales representative for more information. Processing TechniquesNA 336 is specifically designed to provide outstanding drawdown at maximum outputs. The melt strength properties of this resin result in excellent bubble stability. This resin can be processes over a wide range of temperatures; however, recommended conditions are melt temperatures between 300°-330°F and a blow-up ratio between 2.0-2.5:1. Using proper techniques and equipment, drawdown to 0.25 mil is feasible at commercial production rates. Specific recommendations for processing NA 336 can only be made when the processing conditions, equipment and end use are known. For further suggestions, contact your Equistar sales representative.Physical PropertiesThese are typical values and not to be construed as specific product limits. Data obtained from film produced in a 3.5"(89mm) blown film line, commercially available 8"(203 mm)die, 375°F(191°C) melt extrusion temperature, 2:1 BUR, 1.25 mil (32 micron)This product is from the former Equistar product line.
Physical Properties Metric English Comments
Density 0.920 g/cc
0.0332 lb/in³
ASTM D1505
Thickness 31.8 microns
1.25 mil
2.2:1 BUR
Melt Flow 6.5 g/10 min
6.5 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 225 %
225 %
ASTM D882
Film Elongation at Break, TD 450 %
450 %
ASTM D882
Elmendorf Tear Strength MD 350 g
350 g
ASTM D1922
Elmendorf Tear Strength TD 150 g
150 g
ASTM D1922
Dart Drop Test 90.0 g
0.198 lb
F<sub>50</sub>; ASTM D1709
Film Tensile Strength at Break, MD 17.2 MPa
2500 psi
ASTM D882
Film Tensile Strength at Break, TD 13.9 MPa
2020 psi
ASTM D882
1% Secant Modulus, MD 146 MPa
21200 psi
ASTM D882
1% Secant Modulus, TD 165 MPa
24000 psi
ASTM D882
Thermal Properties Metric English Comments
Vicat Softening Point 85.0 °C
185 °F
ASTM D1525
Optical Properties Metric English Comments
Haze 8.0 %
8.0 %
ASTM D1003
Gloss 62 %
62 %
at 45°; ASTM D2457
Processing Properties Metric English Comments
Melt Temperature 163 °C
325 °F
Descriptive Properties Value Comments
Antiblock High
Slip High