Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 17.1 MPa | 2480 psi | ASTM D5035 |
3M GM110 Gripping Material 3M™ Gripping Material GM110 is based on 3M’s proprietary micro-replicated technology. 3M griping material GM 110 consists of a high-friction surface with a nylon knit backing that provides stretch.. |